There is no universal 1:1 conversion factor.
For example, if a mill currently uses:
8 kg Sodium Hydrosulfite / ADT
we would not recommend simply replacing it with 8 kg FAS / ADT.
Instead, conduct a dosage-response test:
Sodium Hydrosulfite:
4 → 6 → 8 → 10 kg/ADT
FAS:
2 → 3 → 5 → 7 → 10 kg/ADT
Then compare:
ISO brightness
Brightness gain
Color reduction
Brightness stability
Pulp strength
Chemical cost / ADT
This produces a much more meaningful replacement ratio.